RELACE MEZI STRUKTUROU, VNITRNIM NAPETIM A RYCHLOSTI CREEPU OCELI FE-21CR-32NI-TI, AL PRI 975 K = RELATION BETWEEN STRUCTURE, INTERNAL STRESS AND CREEP RATE OF A FE-21CR-32NI-TI, AL STEELMILICKA K.1982; KOVOVE MATER.; CSK; DA. 1982-02; VOL. 20; NO 1; PP. 3-9; BIBL. 10 REF.Article
High-temperature transgranular fracture in an austenitic stainless steel = Rupture transgranulaire à haute température d'un acier inoxydable austénitiqueHASEGAWA, T; ILSCHNER, B.Scripta metallurgica. 1983, Vol 17, Num 4, pp 523-527, issn 0036-9748Article
STRUKTURNI KOROZE LEGOVANEHO AUSTENITU PO TEPELNEM ZPRACOVANI = STRUCTURAL CORROSION OF ALLOYED AUSTENITE AFTER HEAT TREATMENTSTEFEC R; FRANZ F; SAFEK V et al.1980; HUTN. LISTY; CSK; DA. 1980-04; VOL. 35; NO 4; PP. 256-261; BIBL. 16 REF.Article
JEHLICOVITA INTRAGRANULARNI FAZE V AUSTENITICKYCH OCELICH NA BAZI FE-21 CR-32 NI V TEPLOTNIM ROZMEZI 975-1075 K = NEEDLE-LIKE INTRAGRANULAR PHASE IN AUSTENITIC FE-21 CR-32NI STEELS WITHIN THE TEMPERATURE INTERVAL 975-1075 KORLOVA A.1980; KOVOVE MATER.; CSK; DA. 1980-08; VOL. 18; NO 4; PP. 417-424; BIBL. 14 REF.Article