Pascal and Francis Bibliographic Databases

Help

Search results

Your search

kw.\*:("ACIERA CR:20-30 NI:20-30 SI:2-2,5")

Publication Year[py]

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Discipline (document) [di]

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Language

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Results 1 to 8 of 8

  • Page / 1
Export

Selection :

  • and

EFFECT OF PRIOR COLD WORKING ON THE CREEP OF 314 ALLOY STEELADELUS JL; GUTTMANN V.1980; MATER. SCI. ENG.; CHE; DA. 1980-07; VOL. 44; NO 2; PP. 195-204; BIBL. 14 REF.Article

PLASMA PREHEATING FOR MACHININGREZNIKOV AN; URITSKIJ ML; KRAVCHENKO SS et al.1981; VESTN. MASINOSTR.; ISSN 0042-4633; SUN; DA. 1981; NO 7; PP. 35-37; BIBL. 4 REF.Article

VLIV OBSAHU KREMIKU NA NACHYLNOST AUSTENITICKYCH CRNI KOROZIVDORNYCH OCELI K MEZIKRYSTALOVE KOROZI = EFFECT OF SILICON CONTENT ON SUSCEPTIBILITY OF AUSTENITIC CORROSION RESISTANT STEELS TO INTERCRYSTALLINE CORROSIONCIHAL V.1980; HUTN. LISTY; CSK; DA. 1980-10; VOL. 35; NO 10; PP. 703-708; BIBL. 20 REF.Article

The kinetics of σ-phase precipitation in AISI 310 and AISI 316 steels = Die Kinetik der σ-Phasenausscheidung in den Staehlen AISI 310 und AISI 316BARCIK, J.Metallurgical transactions. A, Physical metallurgy and materials science. 1983, Vol 14A, Num 4, pp 635-641, issn 0360-2133Article

Initial stages of the high-temperature corrosion of commercial Fe-Cr-Ni alloys in a carburizing atmosphere of low oxygen partial pressure = Etapes initiales de la corrosion à haute température d'alliages commerciaux Fe-Cr-Ni dans une atmosphère carburisante à faible pression partielle d'oxygèneSMITH, P. J; VAN DER BIEST, O; CORISH, J et al.Oxidation of metals. 1985, Vol 24, Num 5-6, pp 277-314, issn 0030-770XArticle

UNTERSUCHUNGEN ZUR WASSERSTOFFVERSPROEDUNG EINIGER KUBISCH-FLAECHENZENTRIERTER WERKSTOFFE = INVESTIGATION INTO HYDROGEN EMBRITTLEMENT OF SOME CUBIC FACE-CENTERED MATERIALSERDMANN JESNITZER F; WESSEL A.1981; ARCH. EISENHUETTENWES.; DEU; DA. 1981-02; VOL. 52; NO 2; PP. 77-82; BIBL. 21 REF.Article

Liquid-solid particle slurry erosion of steels = Stahl-Erosion durch fluessig-fest-Teilchen in SchlammLEVY, A.V; HICKEY, G.Wear. 1987, Vol 117, Num 2, pp 129-146, issn 0043-1648Article

Performance of selected commercial alloys in nitrogen-based sintering atmospheres = Performance d'alliages commerciaux sélectionnés dans des atmosphères de frittage à base d'azoteSMITH, G. D; SEAMS, M. H; FUNKHOUSSER, W. F et al.Progress in powder metallurgy. 1987, Vol 43, pp 441-466, issn 0079-6719Conference Paper

  • Page / 1