Pascal and Francis Bibliographic Databases

Help

Search results

Your search

kw.\*:("ALUMINIUM MAGNESIUM ZINC ALLIAGE")

Publication Year[py]

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Discipline (document) [di]

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Language

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Author Country

A-Z Z-A Frequency ↓ Frequency ↑
Export in CSV

Results 1 to 25 of 68

  • Page / 3
Export

Selection :

  • and

MECHANICAL PROPERTIES OF AL-ZN-MG ALLOYS INVESTIGATED BY MICROHORDNESS MEASUREMENTSJUHASZ A; TASNADI P; KOVACS I et al.1981; J. MATER. SCI.; ISSN 0022-2461; GBR; DA. 1981; VOL. 16; NO 2; PP. 367-372; BIBL. 14 REF.Article

THE CYCLIC STRESS-STRAIN BEHAVIOUR OF AGE-HARDENED CU-CO AND AL-ZN-MG ALLOY SINGLE CRYSTALSWILHELM M.1981; MATER. SCI. ENG.; ISSN 0025-5416; CHE; DA. 1981; VOL. 48; NO 1; PP. 91-106; BIBL. 31 REF.Article

ON THE RELATIONSHIP BETWEEN DUCTILITY AND FRACTURE TOUGHNESS IN AN AL-6.0% ZN-2.5% MG ALLOYKAWABATA T; IZUMI O.1981; ACTA METALL.; ISSN 0001-6160; USA; DA. 1981; VOL. 29; NO 1; PP. 229-239; ABS. FRE/GER; BIBL. 11 REF.Article

The influence of loading frequency on the fatigue crack propagation behaviour of Al-Zn-Mg alloy at low cyclic stress intensity level in 3.5 wt% NaCl solutionYOUNG-GAB CHUN; SUL-IL PYUN; SEONG-MIN LEE et al.Journal of materials science letters. 1991, Vol 10, Num 24, pp 1439-1442, issn 0261-8028Article

PERSISTENT SLIP BANDS IN FATIGUED PEAK AGED AL-ZN-MG SINGLE CRYSTALS. II: PERSISTENT SLIP BANDS IN FRONT OF STAGE I FATIGUE CRACKSVOGEL W; WILHELM M; GEROLD V et al.1982; ACTA METALL.; ISSN 0001-6160; USA; DA. 1982; VOL. 30; NO 1; PP. 31-35; ABS. FRE/GER; BIBL. 18 REF.Article

STRUCTURE CHANGES IN AN AL-4,5 AT.% ZN-2.0 AT.% MG ALLOY DURING CONTINUOUS HEATING IN DEPENDENCE ON THE STARTING CONDITIONSOETTEL GUEFFROY B; LOEFFLER H.1982; CRYSTAL RESEARCH AND TECHNOLOGY (1979); ISSN 0232-1300; DDR; DA. 1982; VOL. 17; NO 11; PP. 1413-1418; ABS. GER; BIBL. 20 REF.Article

DEVELOPMENT OF THE MICROHARDNESS OF AN AL-2.0 AT.% ZN-1.3 AT.% MG ALLOY WITH ADDITIONS OF TECHNICAL IMPURITIES DURING A TWO-STEP AGEING TREATMENT (II)GERLACH R; LOEFFLER H.1982; CRYST. RES. TECHNOL. (1979); ISSN 0232-1300; DDR; DA. 1982; VOL. 17; NO 2; PP. 267-273; ABS. GER; BIBL. 5 REF.Article

A NEUTRON SCATTERING INVESTIGATION OF THE EARLY STAGES OF GUINIER-PRESTON ZONE FORMATION IN ALZNMG (CU)-ALLOYSBLASCHKO O; ERNST G; FRATZL P et al.1982; ACTA METALL.; ISSN 0001-6160; USA; DA. 1982; VOL. 30; NO 2; PP. 547-552; ABS. GER/FRE; BIBL. 11 REF.Article

ON THE INFLUENCE OF THE PRE-AGEING TEMPERATURE ON THE REVERSION BEHAVIOUR OF AN AL-4.5 AT.% ZN-2.0 AT.% MG ALLOYGUEFFROY B; LOEFFLER H.1981; CRYST. RES. TECHNOL.; DDR; DA. 1981; VOL. 16; NO 9; PP. 1079-1085; ABS. GER; BIBL. 17 REF.Article

OXIDATION BEHAVIOUR OF ALUMINIUM ALLOYS CONTAINING MAGNESIUM AND LITHIUMCSANADY A; KURTHY J.1981; J. MATER. SCI.; ISSN 0022-2461; GBR; DA. 1981; VOL. 16; NO 10; PP. 2919-2922; BIBL. 3 REF.Article

INFORMATION GAIN FROM ANALYTICAL DESCRIPTION OF ISOTHERMAL RESISTIVITY CURVESOETTEL W; RADOMSKY C; LOEFFLER H et al.1980; KRIST. TECH.; ISSN 0023-4753; DDR; DA. 1980; VOL. 15; NO 6; PP. 713-719; ABS. GER; BIBL. 14 REF.Article

A MODEL OF THE EFFECT OF R.T. PREAGING ON THE NUCLEATION OF ETA '-PRECIPITATION IN AL-ZN-MG ALLOYSRADOMSKY M; LOEFFLER H; LENDVAI J et al.1980; KRIST. TECH.; ISSN 0023-4753; DDR; DA. 1980; VOL. 15; NO 6; PP. 721-725; ABS. GER; BIBL. 8 REF.Article

ON THE INFLUENCE OF IMPURITY ADDITIONS AND QUENCHING TEMPERATURE ON THE COURSE OF THE MICROHARDNESS (HV) DURING A TWO-STEP AGEING TREATMENT OF AN AL-2.0 AT.%ZN-1.3 AT.%MG ALLOYGERLACH R; LOEFFLER H.1983; CRYSTAL RESEARCH AND TECHNOLOGY (1979); ISSN 0232-1300; DDR; DA. 1983; VOL. 18; NO 3; PP. 367-374; ABS. GER; BIBL. 12 REF.Article

ON THE INFLUENCE OF SHORT R.T. PREAGING ON THE FORMATION OF THE ETA '-PHASE IN AN AL-ZN (4.5 AT.%)-MG (2.5 AT.%) ALLOYRADOMSKY M; LOEFFLER H.1980; KRIST. TECH.; ISSN 0023-4753; DDR; DA. 1980; VOL. 15; NO 6; PP. 703-711; ABS. GER; BIBL. 12 REF.Article

PERSISTENT SLIP BANDS IN FATIGUED PEAK AGED AL-ZN-MG SINGLE CRYSTALS. I: DEVELOPMENT OF DISLOCATION MICROSTRUCTURE AND CHANGE OF PRECIPITATION DISTRIBUTIONVOGEL W; WILHELM M; GEROLD V et al.1982; ACTA METALL.; ISSN 0001-6160; USA; DA. 1982; VOL. 30; NO 1; PP. 21-30; ABS. FRE/GER; BIBL. 16 REF.Article

SERRATED YIELDING AND THE LOCALIZED SHEAR FAILURE MODE IN ALUMINIUM ALLOYSKING JE; YOU CP; KNOTT JF et al.1981; ACTA METALL.; ISSN 0001-6160; USA; DA. 1981; VOL. 29; NO 9; PP. 1553-1566; ABS. FRE/GER; BIBL. 28 REF.Article

ISOTHERMAL AGEING IN THE T RANGE FROM 0OC TO 180OC OF A TECHNICAL AL-2.0 AT.% ZN-1.3 AT.% MG ALLOY AFTER DIRECT QUENCHGERLACH R; LOFFLER H.1982; CRYST. RES. TECHNOL. (1979); ISSN 0232-1300; DDR; DA. 1982; VOL. 17; NO 1; PP. 101-107; ABS. GER; BIBL. 10 REF.Article

ON THE RELATION BETWEEN PRECIPITATION DENSITY AND SIZE AND HARDNESS DURING THE REVERSION TREATMENT OF AN AL-4.5 AT% ZN-2.0 AT% MG ALLOY PRE-AGED AT 100OCGUEFFROY OETTEL B; RAMLAU R; LOFFLER H et al.1982; PHYSICA STATUS SOLIDI. (A). APPLIED RESEARCH; ISSN 0031-8965; DDR; DA. 1982; VOL. 74; NO 1; PP. 149-157; ABS. GER; BIBL. 21 REF.Article

LIQUID-METAL EMBRITTLEMENT IN AN AL 6% ZN 3% MG ALLOYLYNCH SP.1981; ACTA METALL.; ISSN 0001-6160; USA; DA. 1981; VOL. 29; NO 2; PP. 325-340; ABS. FRE/GER; BIBL. 45 REF.Article

ON THE REVERSION BEHAVIOUR OF AN AL-ZN (4.5 AT%)-MG(2.0 AT%) ALLOYGUEFFROY B; LOEFFLER H.1981; PHYS. STATUS SOLIDI (A), APPL. RES.; ISSN 0031-8965; DDR; DA. 1981; VOL. 66; NO 2; PP. 585-590; ABS. GER; BIBL. 22 REF.Article

PRECIPITATION PROCESS IN A CAST ALLOY AL-3.5 WT.PCT ZN-4 WT.PCT MGDZUONG L.1980; KRIST. TECH.; ISSN 0023-4753; DDR; DA. 1980; VOL. 15; NO 6; PP. 697-702; ABS. GER; BIBL. 12 REF.Article

Stage II crack propagation of Al-Zn-Mg-single crystals in dry and wet atmospheresGUDLADT, H.-J; PETIT, J.Scripta metallurgica et materialia. 1991, Vol 25, Num 11, pp 2507-2512, issn 0956-716XArticle

Effects of hydrogen redistribution on hydrogen-assisted cracking in A1-1.% Li and Al-4.5% Zn-2.3% Mg alloysLEE, S.-M; PYUN, S.-I.Scripta metallurgica. 1990, Vol 24, Num 9, pp 1629-1634, issn 0036-9748Article

Hydrogen assisted state I crack propagation in cyclically deformed Al-Zn-Mg single crystalsGUDLADT, H.-J; LENDVAI, J.Scripta metallurgica. 1990, Vol 24, Num 9, pp 1813-1818, issn 0036-9748Article

ETUDE CRISTALLOGRAPHIQUE DE LA PHASE DE TRANSITION M' DANS AL-8%ZN-1%MG = A CRYSTALLOGRAPHIC STUDY OF THE TRANSITION PHASE M' IN AL-8%ZN-1%MG ALLOYREGNIER C; BOUVAIST J; SIMON JP et al.1982; JOURNAL OF APPLIED CRYSTALLOGRAPHY; ISSN 0021-8898; DNK; DA. 1982; VOL. 15; NO 6; PP. 590-593; BIBL. 7 REF.Article

  • Page / 3