Results 1 to 25 of 25

  • Page / 1
Export

Selection :

  • and

LA DEPASSIVATION DES ACIERS INOXYDABLES EN MILIEU NEUTRE.CROLET JL.1977; METAUX CORROS. INDUSTR.; FR.; DA. 1977; VOL. 52; NO 628; PP. 415-422; BIBL. 57 REF.Article

PRESENTATION DES PHENOMENES DE CORROSION ET DES DIFFERENTS MOYENS DE LUTTE DISPONIBLES = DESCRIPTION OF CORROSION PHENOMENA AND DIFFERENT WAYS OF COMBATING THEMCROLET JL.1979; REV. INST. FR. PETROLE; FRA; DA. 1979 PUBL. 1980; VOL. 34; NO 6; PP. 929-946; ABS. ENG/SPA; BIBL. 10 REF.Article

METHODES D'ETUDES DE LA RESISTANCE A LA CORROSION DES ACIERS INOXYDABLES, EXTRAPOLATION DES RESULTATS AUX REALISATIONS INDUSTRIELLESCROLET JL.1978; ACIERS SPEC.; FRA; DA. 1978; NO 42; PP. 21-27; BIBL. 12 REF.Article

UTILISATION DE LA NORME NF A 05-159 POUR LES ESSAIS DE CORROSION INTERGRANULAIRE SUR ACIERS INOXYDABLES AUSTENITIQUES.CROLET JL.1977; COURR. NORM.; FR.; DA. 1977; VOL. 44; NO 258; PP. 455-457; BIBL. 7 REF.Article

LA CORROSION ACIDE DANS LES PUITS (CO2, H2S): ASPECTS METALLURGIQUESCROLET JL.1982; BULL. CENT. RECH. EXPLOR. PROD. ELF-AQUITAINE; ISSN 0396-2687; FRA; DA. 1982; VOL. 2; NO 1; PP. 265-272; ABS. ENG; BIBL. 17 REF.; ILL.Article

METHODES D'ETUDE DE LA RESISTANCE A LA CORROSION DES ACIERS INOXYDABLES. EXTRAPOLATION DES RESULTATS AUX REALISATIONS INDUSTRIELLESCROLET JL.1978; REV. METALLURG.; FRA; DA. 1978; VOL. 75; NO 11; PP. 633-639; BIBL. 12 REF.Article

UTILISATION DES METAUX ET ALLIAGES PASSIVABLES. REGLES DE CHOIX ET EMPLOIS TYPE.CROLET JL.1978; TECHNIQUES DE L'INGENIEUR.; METALLURGIE; FRA; PARIS: TECH. ING.; DA. 1978; NO 74; M153; 12 P.; BIBL. 14 REF.Book Chapter

CRITERES GENERAUX DE RESISTANCE A LA CORROSION DES ACIERS INOXYDABLES: INFLUENCE DE L'ETAT DE SURFACE REELCROLET JL.1976; GENIE CIV.; FR.; DA. 1976; VOL. 151; NO 1; PP. 3-8Article

CRITERES GENERAUX DE RESISTANCE A LA CORROSION DES ACIERS INOXYDABLES; INFLUENCE DE L'ETAT DE SURFACE REELCROLET JL.1976; MATER. ET TECH.; FR.; DA. 1976; VOL. 64; NO 5; PP. 175-181Article

(PH MEASURE OF CO2 AQUEOUS SOLUTIONS UNDER HIGH TEMPERATURE AND HIGH PRESSURE)SSIONBONIS M; CROLET JL.1981; MET., CORROS. IND.; ISSN 0026-1084; FRA; DA. 1981; VOL. 56; NO 675-676; PP. 361-374; ABS. ENG; BIBL. 26 REF.Article

EVALUATION DE LA SUSCEPTIBILITE A LA FRAGILISATION PAR H2S A L'AIDE D'ESSAI DE RUPTURE DIFFEREE SUR EPROUVETTES LISSES CYLINDRIQUES: COMPARAISON ENTRE L'ESSAI NACE NORMAL, L'ESSAI SNEA (P) ET UN ESSAI NACE MODIFIE A PH4 = H2S EMBRITTLEMENT DETERMINATION BY DELAYED FRACTURE TESTING ON CYLINDRICAL TEST PIECES: COMPARISON BETWEEN USUAL NACE, SNEA AND A MODIFIED NACE TESTPERROLLET C; CROLET JL.1982; MEM. ETUD. SCI. REV. METALL.; ISSN 0245-8292; FRA; DA. 1982; VOL. 79; NO 1; PP. 5-14; BIBL. 15 REF.Article

LE ROLE DES IONS ACETATES DANS LA CORROSION PAR CO2 = EFFECT OF ACETATE IONS DURING THE CORROSION BY CO2BONIS M; CROLET JL.1982; MET., CORROS. IND.; ISSN 0026-1084; FRA; DA. 1982; VOL. 57; NO 685; PP. 281-294; ABS. ENG; BIBL. 16 REF.Article

NATURE DU POTENTIEL DE PIQURE DES ACIERS INOXYDABLES. ROLE DES INCLUSIONS ET DES ETATS DE SURFACE.CROLET JL; SERAPHIN L; TRICOT R et al.1977; MEM. SCI. REV. METALLURG.; FR.; DA. 1977; VOL. 74; NO 11; PP. 647-661; BIBL. 1 P. 1/2Article

ACIERS INOXYDABLES RESISTANT A LA CORROSION MARINE.CROLET JL; SERAPHIN L; TRICOT R et al.1977; METAUX CORROS. INDUSTR.; FR.; DA. 1977; VOL. 52; NO 627; PP. 396-405; BIBL. 24 REF.Article

MECANISME D'ACTION DU SOUFRE SUR LA RESISTANCE A LA CORROSION CAVERNEUSE DES ACIERS INOXYDABLES.CROLET JL; SERAPHIN L; TRICOT R et al.1977; MEM. SCI. REV. METALLURG.; FR.; DA. 1977; VOL. 74; NO 5; PP. 281-289; ABS. ALLEM. ANGL. ESP.; BIBL. 21 REF.Article

INFLUENCE DE LA TENEUR EN CHLORURE SUR LE PH DE DEPASSIVATION DES ACIERS INOXYDABLESCROLET JL; SERAPHIN L; TRICOT R et al.1976; MEM. SCI. REV. METALLURG.; FR.; DA. 1976; VOL. 73; NO 1; PP. 1-8; ABS. ALLEM. ANGL. ESP.; BIBL. 11 REF.Article

MECANISME D'ACTION DU SOUFRE SUR LA RESISTANCE A LA CORROSION GENERALE DES ACIERS INOXYDABLES.CROLET JL; SERAPHIN L; TRICOT R et al.1976; METAUX CORROS. INDUSTR.; FR.; DA. 1976; VOL. 51; NO 616; PP. 415-425; BIBL. 22 REF.Article

RESISTANCE A LA CORROSION INTERGRANULAIRE DES ALLIAGES DE TYPE INCOLOY 800 POUR CENTRALES NUCLEAIRESCROLET JL; BILLET R; TRICOT R et al.1976; MEM. SCI. REV. METALLURG.; FR.; DA. 1976; VOL. 73; NO 1; PP. 9-18; ABS. ALLEM. ANGL. ESP.; BIBL. 18 REF.Article

INFLUENCE DES TENEURS EN CHROME, MOLYBDENE ET SOUFRE SUR LA RESISTANCE A LA CORROSION CAVERNEUSE DES ACIERS INOXYDABLESCROLET JL; SERAPHIN L; TRICOT R et al.1975; REV. METALLURG.; FR.; DA. 1975; VOL. 72; NO 12; PP. 937-947; ABS. ALLEM. ANGL. ESP.; BIBL. 6 REF.; (14ES. JOURN. ACIERS SPEC. MEM. TECH.; LUXEMBOURG; 1975)Conference Paper

LIMITE MATHEMATIQUE DE LA METHODE POTENTIOCINETIQUE DE DETERMINATION DU POTENTIEL DE PIQURECROLET JL; SERAPHIN L; TRICOT R et al.1975; C.R. ACAD. SCI., C; FR.; DA. 1975; VOL. 280; NO 6; PP. 333-336; ABS. ANGL.; BIBL. 10 REF.Article

CRITERE ELECTROCHIMIQUE DE RESISTANCE A LA CORROSION: EXEMPLE DU PH DE DEPASSIVATION POUR LA RESISTANCE A LA CORROSION CAVERNEUSE DES ACIERS INOXYDABLESCROLET JL; SERAPHIN L; TRICOT R et al.1978; MATER. ET TECH.; FRA; DA. 1978; VOL. 66; NO 11-12; PP. 355-359; BIBL. 21 REF.Article

MECANISME D'ACTION DU MOLYBDENE SUR LA RESISTANCE A LA CORROSION DE L'ACIER INOXYDABLE 18 CR-2MO RESULFURE.CROLET JL; SERAPHIN L; TRICOT R et al.1976; MEM. SCI. REV. METALLURG.; FR.; DA. 1976; VOL. 73; NO 11; PP. 703-713; ABS. ALLEM. ANGL. ESP.; BIBL. 20 REF.; (JOURN. ACIERS SPEC. 15; SAINT-ETIENNE; 1976)Conference Paper

CARACTERISATION ELECTROCHIMIQUE DE LA RESISTANCE A LA CORROSION CAVERNEUSE DES ACIERS INOXYDABLES: EXEMPLE DES ACIERS FERRITIQUES AU CR-MOCROLET JL; DEFRANOUX JM; SERAPHIN L et al.1975; METAUX CORROS. INDUSTR.; FR.; DA. 1975; VOL. 50; NO 599-600; PP. 262-270; BIBL. 6 REF.Article

CARACTERISATION ELECTROCHIMIQUE DE LA RESISTANCE A LA CORROSION CAVERNEUSE DES ACIERS INOXYDABLESCROLET JL; DEFRANOUX JM; SERAPHIN L et al.1974; MEM. SCI. REV. METALLURG.; FR.; DA. 1974; VOL. 71; NO 12; PP. 797-805; ABS. ANGL. ALLEM. ESP.; BIBL. 22 REF.; (XIIIES. JOURN. ACIERS SPEC.; SAINT-ETIENNE; 1974)Conference Paper

RECHERCHES D'ALLIAGES DE TITANE RESISTANT A LA CORROSIONDE GELAS B; CROLET JL; SERAPHIN L et al.1973; REV. METALLURG.; FR.; DA. 1973; VOL. 70; NO 1; PP. 1-17; ABS. ALLEM. ANGL. ESP.; BIBL. 17 REF.Serial Issue