MACHINING OF HARDENED STEELS WITH CUTTING HEXANITE INSERT TIPSDZHAFAROV AD; EHFENDIEV RM; ZEJNALOV RR et al.1981; HIM. NEFT. MASINOSTR.; ISSN 0023-1126; SUN; DA. 1981; NO 4; PP. 22-23Article

EFFECT OF TOOL BLUNTING CRITER ON CUTTING SPEED OF STEELSKUSHNER VS.1982; VESTN. MASINOSTR.; ISSN 0042-4633; SUN; DA. 1982; NO 2; PP. 64-67; BIBL. 6 REF.Article

THE RESISTANCE OF ELECTROSLAG REMELTED 27GSM AND 33GSM STEELS TO COLD CRACKING IN CO2 WELDING = LA RESISTANCE A LA FISSURATION A FROID DES ACIERS DU TYPE 27GSM ET 33GSM EN SOUDAGE MAGALEKSEENKO VI.1980; WELDG PRODUCT.; ISSN 0043-230X; GBR; DA. 1980; VOL. 27; NO 7; PP. 27-30; BIBL. 3 REF.; DE RUS; LOC. IS;[SVAR PROIZVOD; SUN; DA. 1980; NO 7; PP. 19-20]Article

HYDROGEN EVOLUTION FROM STEELS CONTAINING EPSILON -CU PRECIPITATESISHIZAKI T; TAKEDA T; HIGASHI K et al.1982; J. JAP. INST. MET.; JPN; DA. 1982-01; VOL. 46; NO 1; PP. 28-37; BIBL. 30 REF.Article

DEVELOPMENT OF MANUFACTURING OF CLAD SHEETS AT ZHDANOVSK IRON WORKSBEZNOS VI; NALCHA GI; MEBEL BA et al.1982; METALLURG; SUN; DA. 1982-05; VOL. 27; NO 5; PP. 29-30Article

ERZEUGUNG VON PLATTIERTEN UND HOMOGENEN BLECHEN DURCH WALZEN VON GESCHICHTETEN BLOECKENOVSYANNIKOV VG; SHEVBUNOV EB; SMIRNOV VN et al.1982; METALLURG; SUN; DA. 1982-09; VOL. 27; NO 9; PP. 39-40Article

HOMOGENIZACNI ZIHANI LITE NIZKOLEGOVANE SI-MN-CR-NI-MO OCELI = HOMOGENIZATION ANNEAL OF LOW ALLOYED SI-MN-CR-NI-MO STEELKUCERA J; FORET R; REK A et al.1981; KOVOVE MATER.; CSK; DA. 1981-06; VOL. 19; NO 3; PP. 256-268; BIBL. 8 REF.Article

STACIONARNI MODEL DIFUZE UHLIKU V OKOLI STYKOVCH SVARU. C. 3:ANALYZA DATA NAMERENYCH V SYSTEMU FERIT/AUSTENIT = STEADY STATE MODEL OF CARBON DIFFUSION IN STEEL WELDMENTS. PT. 3KUCERA J; STRANSKY K.1981; KOVOVE MATER.; CSK; DA. 1981-06; VOL. 19; NO 3; PP. 221-233; BIBL. 11 REF.Article

AN ANALYSIS OF STRESS CORROSION CRACK GROWTH BY ANODIC DISSOLUTIONDOIG P; FLEWITT PEJ.1981; METALL. TRANS., A; USA; DA. 1981-06; VOL. 12A; NO 6; PP. 923-931; BIBL. 35 REF.Article

THERMODYNAMIC INVESTIGATION ON THE BEHAVIOR OF BORON IN STEEL CONTAINING AL, TI, N AND CITOH M; SUGIURA S; KONDO K et al.1982; DENKI-SEIKO; JPN; DA. 1982-01; VOL. 53; NO 1; PP. 46-51; BIBL. 7 REF.Article

BESTIMMUNG DER ZAEHIGKEITSMERKMALE DES BRUCHS VON PLATTIERTEN METALLENMAKHUTOV NA; TANANOV AI; CHERNYAEV AP et al.1982; ZAVOD. (LAB); SUN; DA. 1982-01; VOL. 48; NO 1; PP. 66-72; BIBL. 60 REF.Article

HOMOGENIZACNI ZIHANI LITE NIZKOLEGOVANE SI-MN-CR-NI-MO OCELI = HOMOGENIZATION ANNEAL OF LOW ALLOYED SI-MN-CR-NI-MO STEELKUCERA J; FORET R; REK A et al.1981; KOVOVE MATER.; CSK; DA. 1981-06; VOL. 19; NO 3; PP. 256-268; BIBL. 8 REF.Article

STACIONARNI MODEL DIFUZE UHLIKU V OKOLI STYKOVCH SVARU. C. 3:ANALYZA DATA NAMERENYCH V SYSTEMU FERIT/AUSTENIT = STEADY STATE MODEL OF CARBON DIFFUSION IN STEEL WELDMENTS. PT. 3KUCERA J; STRANSKY K.1981; KOVOVE MATER.; CSK; DA. 1981-06; VOL. 19; NO 3; PP. 221-233; BIBL. 11 REF.Article

ON THE STRESS CORROSION CRACK GROWTH RATES OF AISI 4340 STEEL NEAR ITS LOWER TEMPER MARTENSITE EMBRITTLEMENT RANGE IN 0.5 N NACL SOLUTION = UEBER DIE SPANNUNGSKORROSION-RISSWACHSTUMSGESCHWINDIGKEITEN VON STAHL AISI 4340 NAHE DES UNTEREN ANLASSMARTENSIT-VERSPROEDUNGSBEREICHES IN 0,5 N NACL-LOESUNG = SUR LA VITESSE DE CROISSANCE DE CRIQUES DE CORROSION SOUS CONTRAINTE DE LACIER AISI 4340 PRES DE LA REGION INFERIEURE DE FRAGILITE MARTENSITIQUE DE REVENU EN SOLUTION DE NACL 0,5 NTEWARI VK; WINAND R; CHARLIER J et al.1982; ARCH. EISENHUETTENWES.; DEU; DA. 1982-08; VOL. 53; NO 8; PP. 329-333; BIBL. 13 REF.Article

COATINGS OF NITRIDES OF COMPONENTS OF KH18N10T OBTAINED BY KIB PROCESSAKSENOV IM; BREN VG; KUNCHENKO VV et al.1981; FIZ. HIM., OBRAD. MATER.; ISSN 0015-3214; SUN; DA. 1981; NO 5; PP. 100-104; BIBL. 7 REF.Article

GALVANIZING AND GALVANNEALING OF TI-CR-CONTAINING STEEL SHEET FOR DEEP DRAWINGFUKUZUKA T; URAI M; WAKAYAMA K et al.1980; KOBE STEEL ENG. REP., RES. DEV.; JPN; DA. 1980-01; VOL. 30; NO 1; PP. 77-81; BIBL. 8 REF.Article

PRODUCTION OF BIMETALLIC TUBES BY PIERCING AND DRAWING IN DIESAREF'EV VD; ROGOZHIN EH L; DANILIN SI et al.1982; IZVESTIJA VYSSIH UCEBNYH ZAVEDENIJ. CERNAJA METALLURGIJA; ISSN 0368-0797; SUN; DA. 1982; NO 7; PP. 76-79Article

STUDY OF CRISTALLISATION PROCESS IN TWO-LAYER INGOT AFTER ELECTROSLAG POURINGKAZACHKOV EA; MAKUROV SL; ALAKOZOV VF et al.1982; STAL; ISSN 0038-920X; SUN; DA. 1982-08; VOL. 52; NO 8; PP. 48-50; BIBL. 4 REF.Article

INFLUENCE OF ELECTROCHEMICAL POTENTIAL ON CRACK GROWTH RATE BY CORROSION FATIGUE IN SYNTHETIC SEA WATERSAITO T; UCHIYAMA I.1982; TRANS. IRON STEEL INST. JPN.; ISSN 0021-1583; JPN; DA. 1982-08; VOL. 22; NO 8; PP. 586-592; BIBL. 18 REF.Article

INVESTIGATION OF STRESS CORROSION CRACKING OF LOW-ALLOY STEEL IN WATERWU YANG CHU; CHI MEI HSIAO; SHI QUN LI et al.1982; ENG. FRACT. MECH.; GBR; DA. 1982-01; VOL. 16; NO 1; PP. 115-127; BIBL. 7 REF.Article

THE EFFECT OF THE STRESS RATIO ON FATIGUE CRACK GROWTH IN A 3% NACL SOLUTION = EINFLUSS DES SPANNUNGSVERHAELTNISSES AUF DAS ERMUEDUNGSRISSWACHSTUM IN EINER 3%-KOCHSALZLOESUNG = INFLUENCE DE L'ETAT DES CONTRAINTES SUR LA CROISSANCE DES FISSURES DE FATIGUE DANS UNE SOLUTION A 3% DE SEL DE CUISINEKAWAI S.1982; ENG. FRACT. MECH.; GBR; DA. 1982; VOL. 16; NO 6; PP. 857-870; BIBL. 16 REF.Article

TRIBOLOGICAL PROPERTIES OF SOFT METALLIC COATINGS DEPOSITED BY CONVENTIONAL AND THERMIONICALLY ASSISTED TRIODE ION PLATING = PROPRIETES TRIBOLOGIQUES DES REVETEMENTS METALLIQUES MOUS DEPOSES PAR LES METHODES TRADITIONNELLES ET PAR BOMBARDEMENT IONIQUE ASSISTE PAR UNE TRIODE THERMOIONIQUEKLOOS KH; BROSZEIT E; GABRIEL HM et al.1981; THIN SOLID FILMS; ISSN 0040-6090; CHE; DA. 1981; VOL. 80; NO 1-3; PP. 307-319; BIBL. 27 REF.Conference Paper

UEBER DEN EINFLUSS VON TITAN AUF DIE KERBSCHLAGZAEHIGKEIT VON CO2-SCHWEISSGUT = INFLUENCE OF TITANIUM ON THE IMPACT STRENGTH OF CO2 WELD METALMAEDICKE HH; GUTZNER H.1979; ZIS-MITT.; DDR; DA. 1979-09; VOL. 9; PP. 970-976; BIBL. 7 REF.Article

EINFLUSS VON SCHWEFELWASSERSTOFF AUF DAS ZEITSTANDVERHALTEN DES HOEHERFESTEN, SCHWEISSBAREN BAUSTAHLS H 52-3 UND DES KORROSIONSTRAEGEN BAUSTAHLS KT 52-3 = INFLUENCE OF HYDROGEN SULFIDE ON THE RUPTURE BEHAVIOUR OF HIGH-STRENGTH WELDABLE STRUCTURAL STEEL H 53-3 AND CORROSION RESISTANT STRUCTURAL STEEL KT 52-3 = INFLUENCE DE L'HYDROGENE SULFURE SUR LA TENUE DANS LE TEMPS DE L'ACIER DE CONSTRUCTION SOUDABLE DE HAUTE RESISTANCE H 52-3 ET DE L'ACIER DE CONSTRUCTION ANTICORROSION KT 52-3TAUSCHER H; HUNDERTMARK R.1981; IFL-MITT.; DDR; DA. 1981-04; VOL. 20; NO 2; PP. 44-48; BIBL. 13 REF.Article

WEAR MECHANISMS OF COATED CARBIDE TOOLSDEARNLEY PA; TRENT EM.1982; MET. TECHNOL.; GBR; DA. 1982-02; VOL. 9; NO 2; PP. 60-75; BIBL. 23 REF.Article